Aerospace series-Pipe coupling 8 30' in titanium alloy-Thrust wire nuts
Data Sheet by ASD-STAN Standardization, 10/01/2009

Aluminium alloy 7075-T6511 – Bar and section – 1,2 <or= (a or D) <or= 125 mm – With peripheral coarse grain control
Data Sheet by ASD-STAN Standardization, 05/01/1985

Steel FE-PL2105 – Air melted – Hardened and tempered – Bar for machining – De <or= 150 mm – 1 080 MPa <or= Rm <or= 1 280 Mpa
Data Sheet by ASD-STAN Standardization, 11/18/1994

Titanium TI-P99002 – Not heat treated – Grade 2 forging stock, for annealed forgings – a or D <or= 300 mm
Data Sheet by ASD-STAN Standardization, 09/30/1995

Aluminium alloy AL-P2214- T4 – Hand and die forgings – a <or= 100 mm
Data Sheet by ASD-STAN Standardization, 04/30/1998

Carbon fibre reinforced epoxy prepreg – Technical specification – Part 1 : General requirements
Data Sheet by ASD-STAN Standardization, 12/15/1995

Non-metallic materials – Glass tranparencies – Test methods – Determination of modulus of rupture
Data Sheet by ASD-STAN Standardization, 10/31/2001

Titanium TI-P99002 – Annealed – Sheet and strip, hot rolled a <or= 6 mm – 390 MPa <or= Rm <or= 540 MPa
Data Sheet by ASD-STAN Standardization, 04/26/1993

Steel FE-PM3902 (X7CrNiAl17-7) – Air melted – Solution treated and precipitation hardened – Sheet and strip – a <or= 6 mm – 1 240 MPa <or= Rm <or= 1 450 MPa
Data Sheet by ASD-STAN Standardization, 12/31/1997

Steel FE-PM3902 (X7CrNiAl17-7) – Air melted – Solution treated and precipitation hardened – Plate – 6 mm < a <or= 15 mm – 1 240 MPa <or= Rm <or= 1 450 MPa
Data Sheet by ASD-STAN Standardization, 12/31/1997

Aerospace series – Cables, electrical for general purpose single and multicore assembly – XLETFE Family – Part 007: Nickel plated copper – Operating temperatures, between – 65 deg C and 150 deg C – Dual extruded wall for open applications – UV laser printable –
Data Sheet by ASD-STAN Standardization, 07/31/2004

Fluorocarbon rubber (FPM) – Low compression set – Hardness 60 IRHD
Data Sheet by ASD-STAN Standardization, 04/28/1995